MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
BCC Products BC 9040 T Silicone RTV Rubber
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high tear with good elongation. Application: BC9040T is a mold-making material recommended for repetitive production of intricate shapes cast in epoxy or urethane resins. It is also used in the potting of electronic components and in protecting sensitive assemblies against thermal shock and vibration. Deaeration: air entrapped during the mixing cycle must be removed to eliminate voids in the cured compound. Place the mixture in a vacuum of 29 inches of mercury. The mixture will expand to 4-5 times its original volume, crest and recede approximately to its original level. Continue the deaeration for an additional 1-2 minutes and the material will be ready to use. Pouring: pour the silicone material in a continuous stream from approximately 3 inches above the pattern and allow to settle for 5 minutes. Remaining contents are then poured into the mold frame. Adhesion: Two components RTV rubbers show no adhesion to any material except RTV rubbers or conventional silicone rubbers, so primers are required to achieve adhesion to other materials. Storage and Handling: BC 9040T base and Catalyst-BC 9040T will remain useful for six (6) months from date of shipment when stored in their original unopened containers in a dry place at or below 80 ºF. Avoid contact of Catalyst-BC 9040T with acidic bases and oxidizing materials as such can generate flammable gas.

Information provided by BCC Products, Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Brookfield Viscosity, Catalyst
  • Brookfield Viscosity, Mixed
  • Brookfield Viscosity, Compound
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tear Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • Cure Time
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.