MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products BC 9040 T Silicone RTV Rubber
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high tear with good elongation. Application: BC9040T is a mold-making material recommended for repetitive production of intricate shapes cast in epoxy or urethane resins. It is also used in the potting of electronic components and in protecting sensitive assemblies against thermal shock and vibration. Deaeration: air entrapped during the mixing cycle must be removed to eliminate voids in the cured compound. Place the mixture in a vacuum of 29 inches of mercury. The mixture will expand to 4-5 times its original volume, crest and recede approximately to its original level. Continue the deaeration for an additional 1-2 minutes and the material will be ready to use. Pouring: pour the silicone material in a continuous stream from approximately 3 inches above the pattern and allow to settle for 5 minutes. Remaining contents are then poured into the mold frame. Adhesion: Two components RTV rubbers show no adhesion to any material except RTV rubbers or conventional silicone rubbers, so primers are required to achieve adhesion to other materials. Storage and Handling: BC 9040T base and Catalyst-BC 9040T will remain useful for six (6) months from date of shipment when stored in their original unopened containers in a dry place at or below 80 ºF. Avoid contact of Catalyst-BC 9040T with acidic bases and oxidizing materials as such can generate flammable gas.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 1000 cPCatalyst
 38000 cPMixed
 52000 cP
@Temperature 25.0 °C
Compound
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength, Ultimate 750 psi
Elongation at Break 375 %
Tear Strength 85.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 3.1
@Frequency 100 Hz
Dielectric Strength 584 V/mil
Dissipation Factor 0.0010
@Frequency 100 Hz
Arc Resistance 180 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 90.0 min
@Temperature 60.0 °C
Pot Life 90 min
@Temperature 25.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Mix Ratio10:1 by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Humiseal 1C49 Silicone Conformal Coating
NuSil R21-2615 Silicone Two Part Sealing & Adhesive
Wacker Lumisil® LR 7601/80 Liquid Silicone Rubber

PBCC059 / 107286

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.