MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SEKISUI SPI KYDEX® XD Thermoplastic 3D Laminate
Categories: Polymer; Thermoplastic

Material Notes: For flat lamination and membrane pressed applications

KYDEX® XD is a thermoplastic 3D laminate giving designers the ability to incorporate compound corners, logos, and wire management holes while eliminating unsightly seams and the need for edgebanding typically associated with HPL/TFM surfaces. Its integral color and superior impact resistance minimizes costly maintenance associated with other laminates.

Extreme durability (XD), superior impact, membrane pressable thermoplastic 3D laminate with integral color from 0.76 mm - 1.02 mm (0.030 in - 0.040 in) thickness. While providing god definition it surpasses vinyl overlays, high pressure laminates and melamine in resistance to surface and edge impact.

Suggested Applications

  • Store fixtures
  • Checkout counters
  • Exhibits and displays
  • Moldings
  • Transaction surfaces
  • Workstations
  • Logo and trademark panels
  • Kiosks
  • Cabinetry
  • Door and drawer fascias
  • Pedestals and stands
  • Gondolas
  • Tabletops
  • Flat laminated panels

Features:

  • Tough and durable
  • Resistant to cracking and chipping
  • Solid, integral color
  • 3500+ custom colors
  • Resistant to a wide range of chemicals
  • Abrasion resistant
  • Fire retardant
  • Excellent fabrication qualities
  • Very low moisture absorption
  • Membrane pressable
  • Flexibility allows small radius bends

Values based upon 3.20 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Modulus of Elasticity, ASTM D790
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Impact Test, NEMA LD3 - 2005, Dart Impact Resistance; Unitless
  • Abrasion, ASTM D1044, Type CS10F wheel
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D658, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D658, Annealed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.