MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® XD Thermoplastic 3D Laminate
Categories: Polymer; Thermoplastic

Material Notes: For flat lamination and membrane pressed applications

KYDEX® XD is a thermoplastic 3D laminate giving designers the ability to incorporate compound corners, logos, and wire management holes while eliminating unsightly seams and the need for edgebanding typically associated with HPL/TFM surfaces. Its integral color and superior impact resistance minimizes costly maintenance associated with other laminates.

Extreme durability (XD), superior impact, membrane pressable thermoplastic 3D laminate with integral color from 0.76 mm - 1.02 mm (0.030 in - 0.040 in) thickness. While providing god definition it surpasses vinyl overlays, high pressure laminates and melamine in resistance to surface and edge impact.

Suggested Applications

  • Store fixtures
  • Checkout counters
  • Exhibits and displays
  • Moldings
  • Transaction surfaces
  • Workstations
  • Logo and trademark panels
  • Kiosks
  • Cabinetry
  • Door and drawer fascias
  • Pedestals and stands
  • Gondolas
  • Tabletops
  • Flat laminated panels

Features:

  • Tough and durable
  • Resistant to cracking and chipping
  • Solid, integral color
  • 3500+ custom colors
  • Resistant to a wide range of chemicals
  • Abrasion resistant
  • Fire retardant
  • Excellent fabrication qualities
  • Very low moisture absorption
  • Membrane pressable
  • Flexibility allows small radius bends

Values based upon 3.20 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength 42.0 MPaASTM D638
Elongation at Break 126 %ASTM D638
Modulus of Elasticity 2.48 GPaASTM D790
Tensile Modulus 2416 MPaASTM D638
Flexural Strength 66.0 MPaASTM D790
Izod Impact, Notched 801 J/mASTM D256
Impact Test >= 1000 in-lb
@Thickness 1.02 mm
Dart Impact Resistance; Unitless; NEMA LD3 - 2005
Abrasion 9.5
@Load 0.500 kg
Type CS10F wheel; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 151 °FUnannealed; ASTM D658
 168 °FAnnealed; ASTM D658
 
Descriptive Properties
Ball Test>3000NEMA LD3 - 2005; Impact Resistance; Thickness: 0.040 in (1.02 mm)
Cleanability16NEMA LD3 - 2005
Surface Burning CharacteristicsClass 1/AASTM E84; Flame Spread/Smoke; Thickness: 0.040 in (1.02 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 6513 Thermoplastic
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 4545 Thermoplastic

PSEKIS050 / 185875

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.