MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excellent sealing material with a very low seal initiation temperature and high clarity.

Availability: Latin America, North America and South America

Applications:

  • Adhesive Lamination
  • Barrier Food Packaging
  • Coextrusion Coating
  • Compounding
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Flexible Packaging
  • High Frequency Sealing
  • Industrial Packaging
  • Injection Molding
  • Masterbatch Base Resin
  • Non-woven Coating
  • PVC Replacement
  • Thermal Lamination
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors:
Available Properties
  • Density, ExxonMobil method
  • Vinyl Acetate Content, ExxonMobil method
  • Melt Flow, ASTM D1238
  • Neck In, ExxonMobil Method, 656 ft/min, constant output at 35 rpm
  • Neck In, ExxonMobil Method, 328 ft/min, constant output at 35 rpm
  • Drawdown, ExxonMobil Method, Constant output at 35 rpm
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Film Elongation at Break, MD, ASTM D882
  • Film Tensile Strength at Break, MD, ASTM D882
  • Melting Point, ExxonMobil method, Peak Melting Point
  • Vicat Softening Point, ASTM D1525
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.