Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excellent sealing material with a very low seal initiation temperature and high clarity. Availability: Latin America, North America and South America Applications: - Adhesive Lamination
- Barrier Food Packaging
- Coextrusion Coating
- Compounding
- Document Plastification
- Extrusion Coating
- Extrusion Lamination
- Flexible Packaging
- High Frequency Sealing
- Industrial Packaging
- Injection Molding
- Masterbatch Base Resin
- Non-woven Coating
- PVC Replacement
- Thermal Lamination
- Wire and Cable Compounds
Information provided by ExxonMobil |