MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Michelman® Michem® Coat 95 Water and grease resistant, heat sealable coating
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Water and grease resistant, heat sealable coating

Usage: Michem® Coat 95 is a good multi-purpose coating that provides excellent water, oil and grease resistance. This product is heat sealable and cold set gluable as well.

Application data: Michem®Coat 95 is designed to be flexo or gravure applicable. For use as a heat seal coating on paper at a dry coating weight between 4 - 6gsm is recommended. Typical sealing conditions are 140-200C, 4 bar pressure, 1 sec dwell time.

Michem® Coat is typically used for: Bakery products; Packaged butter; Pizza boxes; Machinery: Electrical components; Metal parts and Sensitive papers

Food Contact Information when manufactured in Belgium:
FDA:
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods
176.180: Components of paper and paperboard in contact with dry foods

Information provided by Michelman®

Vendors:
Available Properties
  • Specific Gravity
  • pH
  • Brookfield Viscosity, Spindle # 3, rpm 20
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.