MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Michelman® Michem® Coat 95 Water and grease resistant, heat sealable coating
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Water and grease resistant, heat sealable coating

Usage: Michem® Coat 95 is a good multi-purpose coating that provides excellent water, oil and grease resistance. This product is heat sealable and cold set gluable as well.

Application data: Michem®Coat 95 is designed to be flexo or gravure applicable. For use as a heat seal coating on paper at a dry coating weight between 4 - 6gsm is recommended. Typical sealing conditions are 140-200C, 4 bar pressure, 1 sec dwell time.

Michem® Coat is typically used for: Bakery products; Packaged butter; Pizza boxes; Machinery: Electrical components; Metal parts and Sensitive papers

Food Contact Information when manufactured in Belgium:
FDA:
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods
176.180: Components of paper and paperboard in contact with dry foods

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.10 g/cc
pH 7.0 - 9.0
Brookfield Viscosity 300 - 750 cPSpindle # 3, rpm 20
 
Descriptive Properties
AppearanceOff-white liquid
Solids TypeAcrylic Styrene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHEL063 / 134980

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.