MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Envalior Arnitel® ID 2045 Copolyester, >50% Renewable Content, 3D Printing Grade
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: This is a filament grade - not available for sale as granules.

Arnitel® ID 2045 is a highly flexible TPC (thermoplastic copolyester) that can be used in a broad range of applications from sports mouth guards to electronics. It is a flexible polymer with very good UV- and chemical-resistance compared to other flexible polymers such as TPU (thermoplastic urethane).

Arnitel® ID 2045 is an ECO label filament made with 50% bio-based feedstock which passes USP class IV, ISO 10993-10 Irritation / Intracutaneous reactivity as well as ISO 10993-5 Cytotoxicity tests. It combines easy and fast printing with high performance characteristics enabled by excellent inter-layer adhesion due to its slower crystallization behavior.

The mechanical data is tested on printed tensile bars, printed in two directions: 0°-90° and 45°-45°

The material passed the ISO irritation, ISO cytotoxicity and the USP VI tests.

Sustainability: Bio-based - 14C measurable

Special features: Contains renewable content

Processing technology: 3D printing

Former DSM Engineering Plastics product line is now with Envalior.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62
  • Moisture Absorption, Sim. to ISO 62
  • Melt Flow, ISO 1133, Melt Volume-Flow Rate (cm3/10 min)
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Tensile Strength at Break, ISO 527-1/-2, 3D printed tensile bars, 0°-90°
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2, 3D printed tensile bars, 0°-90°
  • Elongation at Break, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Tensile Modulus, ISO 527-1/-2, 3D printed tensile bars, 0°-90°
  • Tensile Modulus, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Tear Strength, ISO 34-1; Method B
  • Volume Resistivity, IEC 60093
  • Surface Resistivity per Square, IEC 60093
  • Dielectric Strength, IEC 60243-1
  • Melting Point, ISO 11357-1/-3, 10°C/min
  • Vicat Softening Point, ISO 306, 50°C/h
  • Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min
  • Flammability, UL94, IEC 60695-11-10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Envalior, former LANXESS

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.