MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and cement and steel-mill equipment. Resistant to the effects of seizing or galling, low coefficient of friction alloys sliding contact with other metals. Used in equipment where no lubricants are used. Outstanding resistance to cavitation-erosion. Combines wear and corrosion resistance with good impact strength and resistance to thermal shock. Retains high hardness, even at red heat. Electrical conductivity 1.90% compared to Copper. 2360 MPa average modulus of rupture of sheet at room temperature. Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Mutual indentation method
  • Hardness, Brinell, Mutual indentation method
  • Hardness, Brinell, Mutual indentation method
  • Hardness, Brinell, Mutual indentation method
  • Hardness, Knoop, Converted from Brinell Hardnesses
  • Hardness, Knoop, Converted from Brinell Hardnesses
  • Hardness, Knoop, Converted from Brinell Hardnesses
  • Hardness, Knoop, Converted from Brinell Hardnesses
  • Hardness, Rockwell A, Converted from Brinell Hardnesses
  • Hardness, Rockwell A, Converted from Brinell Hardnesses
  • Hardness, Rockwell A, Converted from Brinell Hardnesses
  • Hardness, Rockwell A, Converted from Brinell Hardnesses
  • Hardness, Rockwell B, Converted from Brinell Hardnesses
  • Hardness, Rockwell B, Converted from Brinell Hardnesses
  • Hardness, Rockwell B, Converted from Brinell Hardnesses
  • Hardness, Rockwell B, Converted from Brinell Hardnesses
  • Hardness, Vickers, Converted from Brinell Hardnesses
  • Hardness, Vickers, Converted from Brinell Hardnesses
  • Hardness, Vickers, Converted from Brinell Hardnesses
  • Hardness, Vickers, Converted from Brinell Hardnesses
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Modulus of Elasticity, sheet at RT
  • Modulus of Elasticity, bar
  • Izod Impact Unnotched, plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
  • Charpy Impact, Longitudinal
  • Charpy Impact, Longitudinal
  • Charpy Impact, Unnotched, Transverse
  • Charpy Impact, Unnotched, Longitudinal
  • Charpy Impact, Unnotched, Longitudinal
  • Charpy Impact, Unnotched, Longitudinal
  • Charpy Impact, Unnotched, Longitudinal
  • Electrical Resistivity
  • Magnetic Permeability, 200 Oersted (15.900 A/m)
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity, at RT (calculated)
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Reflection Coefficient, Visible (0-1), reflecting power
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Kennametal Stellite, former Deloro Stellite Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.