Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good processabilityApplications: automotive claddings and rocker panels, grilles, appliques Description: Hifax ETA-3163 medium melt flow, paintable, minearl-filled thermoplastic elastoeric olefin resin has an excellent balance of stiffness, low temperature impact resistance and dimensional stability. It was designed specifically for use in varoius automotive exterior ornamentation applications. Information provided by Montell Polyolefins. LyondellBasell is the successor company to Montell. |