MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good processability

Applications: automotive claddings and rocker panels, grilles, appliques

Description: Hifax ETA-3163 medium melt flow, paintable, minearl-filled thermoplastic elastoeric olefin resin has an excellent balance of stiffness, low temperature impact resistance and dimensional stability. It was designed specifically for use in varoius automotive exterior ornamentation applications.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Linear Mold Shrinkage 0.010 cm/cmTool, Montell
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 40ISO 2039-2
Hardness, Shore D 64ISO 686
Tensile Strength, Ultimate 14.0 MPaISO R527-1
Tensile Strength, Yield 17.0 MPaISO R527-1
Elongation at Break 350 %ISO R527-1
Elongation at Yield 7.0 %ISO R527-1
Flexural Modulus 1.00 GPaISO 178
Izod Impact, Notched 0.660 J/cm
@Temperature -40.0 °C
ISO 180
Impact Test 25.0 J
@Temperature -30.0 °C
MAII, E at Max Load, Ductile; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °CISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
LyondellBasell Hifax™ TRA-3263EC/1 Thermoplastic Olefin Resin
LyondellBasell Hifax™ CJ232 Thermoplastic Olefin Resin
LyondellBasell Hifax™ CB229 Thermoplastic Olefin Resin

PMO480 / 53649

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.