MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
BYK ADD-VANCE® Cleaning Masterbatch  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fields of application: Cleaning masterbatch for thermoplastic materials like olefins and styrenics. To be used in extruders and die-systems for all film- and filament / fibers lines as well as injection- and blow molding processes.
Examples: Purging material for cleaning the extruder e.g. for color changes, removal of black spots and degraded polymer

Mode of action and advantages: ADD-VANCE® Cleaning is a ready-for-use non-toxic cleaning masterbatch. Degraded production polymer, additives and pigments will swell due to reactions with ADD-VANCE® Cleaning. As a result impurities will loose from the metal parts and be removed from the machinery.

Advantages: Excellent cleaning of extruder parts; Effectively removes black spots in one or two cleaning operations. Only a small amount of cleaning material is needed. Cost-effective cleaning masterbatch; Saves time and energy for the cleaning operation. Reduction of machine downtime; Penetrates effectively into all dead areas of extruder and die. Shorter start-up periods; Can be processed like general thermoplastic granules, processing conditions (temperatures) do not need to be changed; Non-sticking pellets, dust free dosing; Safe and easy handling, will not damage cylinder, screw, die, and nozzle systems of the machines, even when used repeatedly; and Using ADD-VANCE® Cleaning is the last remedy to remove black spots before taking an extruder apart (pulling the screw).

Former ADDCOMP product line, acquired by BYK.

Vendors:
Available Properties
  • Bulk Density
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Former Addcomp

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.