MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Solaxis FDM Nylon 12CF 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: FDM Nylon 12CF™ is a carbon-filled thermoplastic with excellent structural characteristics. The material is comprised of a blend of Nylon 12 resin and chopped carbon fiber, at a loading of 35% by weight. This combination produces one of the strongest thermoplastics in the FDM® material portfolio. It has the highest flexural strength of any FDM thermoplastic, resulting in the highest stiffness-to-weight ratio. Appropriate uses include strong but lightweight tooling applications and functional prototypes in the aerospace, automotive, industrial and recreational manufacturing industries. FDM Nylon 12CF is available on the Fortus 450mc™ and Stratasys F900™ 3D Printers and is compatible with SR-110™ support material.

Information provided by Solaxis Ingenious Manufacturing

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Tensile Strength, Ultimate, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Strength, Ultimate, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Flexural Strength, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Flexural Strength, ASTM D790, XZ Axis, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, XZ Axis, Method 1, 0.05 in./min
  • Flexural Strain at Break, ASTM D790, XZ Axis, Method 1, 0.05 in./min
  • Flexural Strain at Break, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Compressive Strength, ASTM D695, Ultimate, XZ Axis, Method 1, 0.05"/min
  • Compressive Strength, ASTM D695, Ultimate, ZX Axis, Method 1, 0.05"/min
  • Compressive Modulus, ASTM D695, ZX Axis, Method 1, 0.05"/min
  • Compressive Modulus, ASTM D695, XZ Axis, Method 1, 0.05"/min
  • Izod Impact, Notched, ASTM D256, ZX Axis, Method A
  • Izod Impact, Notched, ASTM D256, XZ Axis, Method A
  • Izod Impact, Unnotched, ASTM D256, ZX Axis, Method A
  • Izod Impact, Unnotched, ASTM D256, XZ Axis, Method A
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.