MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Solaxis FDM Nylon 12CF 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: FDM Nylon 12CF™ is a carbon-filled thermoplastic with excellent structural characteristics. The material is comprised of a blend of Nylon 12 resin and chopped carbon fiber, at a loading of 35% by weight. This combination produces one of the strongest thermoplastics in the FDM® material portfolio. It has the highest flexural strength of any FDM thermoplastic, resulting in the highest stiffness-to-weight ratio. Appropriate uses include strong but lightweight tooling applications and functional prototypes in the aerospace, automotive, industrial and recreational manufacturing industries. FDM Nylon 12CF is available on the Fortus 450mc™ and Stratasys F900™ 3D Printers and is compatible with SR-110™ support material.

Information provided by Solaxis Ingenious Manufacturing

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 34.4 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 75.6 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Strength, Yield 28.8 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 63.4 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Break 1.2 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 1.9 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Yield 0.90 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
 1.1 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Modulus 2.30 GPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 7.50 GPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Flexural Strength 58.1 MPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 142 MPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Modulus 1.83 GPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 10.62 GPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Strain at Break >= 3.0 %XZ Axis, Method 1, 0.05 in./min; ASTM D790
 >= 3.0 %ZX Axis, Method 1, 0.05 in./min; ASTM D790
Compressive Strength 67.0 MPaUltimate, XZ Axis, Method 1, 0.05"/min; ASTM D695
 92.0 MPaUltimate, ZX Axis, Method 1, 0.05"/min; ASTM D695
Compressive Modulus 2.17 GPaZX Axis, Method 1, 0.05"/min; ASTM D695
 2.67 GPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Izod Impact, Notched 21.4 J/mZX Axis, Method A; ASTM D256
 85.0 J/mXZ Axis, Method A; ASTM D256
Izod Impact, Unnotched 85.0 J/mZX Axis, Method A; ASTM D256
 310 J/mXZ Axis, Method A; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 140000 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 33000 - 690000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 40.0 °C
ASTM E831
 27.0 µm/m-°C
@Temperature 100 °C
ASTM E831
CTE, linear, Transverse to Flow 150 µm/m-°C
@Temperature 40.0 °C
ASTM E831
 300 µm/m-°C
@Temperature 100 °C
ASTM E831
Melting Point 178 °C
Deflection Temperature at 1.8 MPa (264 psi) 143 °CASTM D648
Glass Transition Temp, Tg 41.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLXIS986 / 256143

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.