Temper: As Centrifugal Cast Casting Characteristics: High – Effect of Section Size, Fluidity; Med-High – Gassing; Medium – Casting Yield; Low - Drossing, Shrinkage in Solidification Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding Typical uses: Bearings; Bearings for Heavy Loads and Relatively Low Speeds; Gear Boxes; Gears; Restaurant Equipment; Speed Reducers; Valve Bodies; Worm Gears; Worm Wheels Applicable Specifications: As Centrifugal Cast – Castings SAE J462; Castings SAE J461, Castings ASTM B427; As Continuous Cast – Castings ASTM B505/B505M, Castings SAE J462, Castings SAE J461; As Sand Cast – Castings SAE J461, Castings SAE J462, Castings B427; Ingot - ASTM B30 |