MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tin Bronze, UNS C90700, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Effect of Section Size, Fluidity; Med-High – Gassing; Medium – Casting Yield; Low - Drossing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Bearings; Bearings for Heavy Loads and Relatively Low Speeds; Gear Boxes; Gears; Restaurant Equipment; Speed Reducers; Valve Bodies; Worm Gears; Worm Wheels

Applicable Specifications: As Centrifugal Cast – Castings SAE J462; Castings SAE J461, Castings ASTM B427; As Continuous Cast – Castings ASTM B505/B505M, Castings SAE J462, Castings SAE J461; As Sand Cast – Castings SAE J461, Castings SAE J462, Castings B427; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.317 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 95
@Load 500 kg
for Standard
 102
@Load 500 kg
Tensile Strength >= 50.0 ksifor Standard
 55.0 ksiTypical
Tensile Strength, Yield >= 28.0 ksifor Standard, 0.5% Ext
 30.0 ksiTypical, 0.5% Ext
Elongation at Break >= 12 %for Standard
 16 %Typical
Tensile Modulus 15000 ksi
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000172 ohm-cm10% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.2 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 40.8 BTU-in/hr-ft²-°F
Melting Point 1528 - 1830 °F
Solidus 1528 °F
Liquidus 1830 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.20 %
Copper, Cu 88 - 90 %
Iron, Fe <= 0.15 %
Lead, Pb <= 0.50 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 0.30 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.050 %
Tin, Sn 10 - 12 %
Zinc, Zn <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC90700x1 / 293193

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.