MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Saint-Gobain Versilon™ C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Formerly Tygothane® C-544-AI.B.. This Pressure Tubing can be used in some of the most physically demanding applications, such as those requiring a tight bend radius. Specially formulated from tough, ether-based polyurethane resin, Tygothane® Pressure Tubing is resistant to a range of chemicals, including oils, greases, solvents and chemicals. Because of its excellent wear properties, Tygothane® Pressure Tubing frequently outperforms traditional rubber, plastic and metal materials when exposed to abrasive conditions. Tygothane® Pressure Tubing is also plasticizer free, and remains flexible even when cycled through temperature extremes.

Features/Benefits:
  • Exceptional abrasion and tear resistance
  • Tough braid reinforcement for elevated working pressures
  • Excellent resistance to oils, greases and fuels
  • Retains flexibility in sub-zero environments
  • Ideal for use with Tygopure™ reusable fittings
  • Meets FDA and NSF 51 criteria for food contact
  • Meets NSF 61 criteria for potable water contact
Typical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792-91
  • Water Absorption, ASTM D570-81, 24 hours at 23°C
  • Hardness, Shore A, ASTM D2240-91, 15 seconds
  • Tensile Strength, Yield, ASTM D412-92
  • Elongation at Break, ASTM D412-92
  • 100% Modulus, ASTM D412-92
  • 300% Modulus, ASTM D412-92
  • Tear Strength, ASTM D1004-93, Initial Tear Strength
  • Compression Set, ASTM D395-89 Method B, Constant Deflection, for 22 hrs.
  • Tensile Set, ASTM D412-92
  • Dielectric Strength, ASTM D149-93
  • Maximum Service Temperature, Air
  • Brittleness Temperature, ASTM D746-79
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.