MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Versilon™ C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Formerly Tygothane® C-544-AI.B.. This Pressure Tubing can be used in some of the most physically demanding applications, such as those requiring a tight bend radius. Specially formulated from tough, ether-based polyurethane resin, Tygothane® Pressure Tubing is resistant to a range of chemicals, including oils, greases, solvents and chemicals. Because of its excellent wear properties, Tygothane® Pressure Tubing frequently outperforms traditional rubber, plastic and metal materials when exposed to abrasive conditions. Tygothane® Pressure Tubing is also plasticizer free, and remains flexible even when cycled through temperature extremes.

Features/Benefits:
  • Exceptional abrasion and tear resistance
  • Tough braid reinforcement for elevated working pressures
  • Excellent resistance to oils, greases and fuels
  • Retains flexibility in sub-zero environments
  • Ideal for use with Tygopure™ reusable fittings
  • Meets FDA and NSF 51 criteria for food contact
  • Meets NSF 61 criteria for potable water contact
Typical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792-91
Water Absorption 1.8 %24 hours at 23°C; ASTM D570-81
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8515 seconds; ASTM D2240-91
Tensile Strength, Yield 5000 psiASTM D412-92
Elongation at Break 400 %ASTM D412-92
100% Modulus 0.800 ksi
@Strain 100 %
ASTM D412-92
300% Modulus 1.20 ksi
@Strain 300 %
ASTM D412-92
Tear Strength 350 pliInitial Tear Strength; ASTM D1004-93
Compression Set 19 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 45 %ASTM D412-92
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 550 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Brittleness Temperature -100 °FASTM D746-79
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Versilon™ C-210-A Precision Polyurethane Tubing Formulation

PSTGQZ203 / 68717

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.