MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Amodel® AS-1935 HS PPA, 35% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: 35% glass fiber, for thick-wall parts (>3mm), glycol resistant, heat stabilized, lubricated

Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material exceeds the performance required by the automotive industry for polymeric materials exposed to antifreeze at 226°F (108°C), even when tested at 275°F (135°C).

- Black: AS-1935 HS BK 328

Applications: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts

Features: Antifreeze Resistant; Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Glycol Resistance; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength

Injection notes: Mold Temperature:
- Higher tool temperatures might be required for thin wall sections
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ISO 1183, Method A
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength at Break, ISO 527-2
  • Elongation at Break, ASTM D638
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2, 1 mm/min, Type 1A
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180, Type 1, Notch A
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Volume Resistivity, IEC 62631-3-1
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed, Flatwise
  • Flammability, UL94
  • Oxygen Index, ISO 4589-2
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Feed Temperature, Injection Hopper
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Moisture Content, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.