MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AS-1935 HS PPA, 35% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: 35% glass fiber, for thick-wall parts (>3mm), glycol resistant, heat stabilized, lubricated

Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material exceeds the performance required by the automotive industry for polymeric materials exposed to antifreeze at 226°F (108°C), even when tested at 275°F (135°C).

- Black: AS-1935 HS BK 328

Applications: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts

Features: Antifreeze Resistant; Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Glycol Resistance; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength

Injection notes: Mold Temperature:
- Higher tool temperatures might be required for thin wall sections
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccMethod A; ISO 1183
Water Absorption 0.10 %
@Thickness 4.00 mm,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 205 MPaASTM D638
 210 MPaISO 527-2
Elongation at Break 2.2 %ASTM D638
 2.2 %ISO 527-2
Tensile Modulus 12500 MPaASTM D638
 12600 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 275 MPaASTM D790
 300 MPaISO 178
Flexural Modulus 11300 MPaASTM D790
 11500 MPaISO 178
Izod Impact, Notched 65.0 J/mASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²Type 1, Notch A; ISO 180
Charpy Impact Unnotched 66.0 kJ/m²ISO 179
Charpy Impact, Notched 8.00 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 7.60 kJ/m²
@Temperature -30.0 °C
Type 1, Edgewise, Notch A; ISO 179
 8.60 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 7.20e+15 ohm-cmIEC 62631-3-1
Surface Resistance 5.20e+15 ohmIEC 60093
Dielectric Constant 3.59
@Frequency 1e+6 Hz
IEC 60250
 3.85
@Frequency 100000 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 100000 Hz
IEC 60250
 0.013
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.20 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2
 17.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 56.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-2
 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2
 110 µm/m-°C
@Temperature 55.0 - 125 °C
ISO 11359-2
Melting Point 323 °CISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °CUnannealed, Flatwise; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.900 mm
Oxygen Index 24 %ISO 4589-2
Glow Wire Ignition Temperature 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.20 mm
IEC 60695-2-13
 725 °C
@Thickness 0.900 mm
IEC 60695-2-13
Glow Wire Flammability Index 675 °C
@Thickness 1.50 mm
IEC 60695-2-12
 700 °C
@Thickness 0.900 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 79.0 °CInjection Hopper
Rear Barrel Temperature 310 - 330 °C
Middle Barrel Temperature 315 - 330 °C
Front Barrel Temperature 325 - 335 °C
Melt Temperature 320 - 345 °CInjection
Mold Temperature 150 °C
Drying Temperature 121 °C
@Time 14400 sec
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4087 / 279887

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.