MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
3M Scotch™ 130C Linerless Rubber Splicing Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice heat. The tape is designed for use in splicing and terminating wires and cables. Rated up to 90°C continuous operating temperatures and short-term 130°C overload service. The tape has excellent physical and electrical properties, which provide immediate moisture seals and void-free build-ups. The product can be used for low and high-voltage (through 69 kV) applications.

Information provided by 3M

Vendors:
Available Properties
  • Thickness
  • Tensile Strength at Break, ASTM D4325
  • Elongation at Break, ASTM D4325
  • Volume Resistivity, ASTM D4325, Aged 96 hrs at 96% RH
  • Volume Resistivity, ASTM D4325, Original
  • Dielectric Constant, ASTM D4325, 1200V
  • Dielectric Constant, ASTM D4325, 1200V
  • Dielectric Strength, ASTM D4325, 96 hrs at 96% RH
  • Dielectric Strength, ASTM D4325, Original
  • Dielectric Strength, ASTM D4325, 24 hrs in water
  • Dissipation Factor, ASTM D4325, 1200V
  • Thermal Conductivity, ASTM C518
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Emergency Overload
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.