MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch™ 130C Linerless Rubber Splicing Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice heat. The tape is designed for use in splicing and terminating wires and cables. Rated up to 90°C continuous operating temperatures and short-term 130°C overload service. The tape has excellent physical and electrical properties, which provide immediate moisture seals and void-free build-ups. The product can be used for low and high-voltage (through 69 kV) applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 30.0 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1.72 MPaASTM D4325
Elongation at Break 850 %ASTM D4325
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmAged 96 hrs at 96% RH; ASTM D4325
 >= 1.00e+15 ohm-cmOriginal; ASTM D4325
Dielectric Constant 3.5
@Frequency 60.0 Hz,
Temperature 23.0 °C
1200V; ASTM D4325
 3.6
@Frequency 60.0 Hz,
Temperature 90.0 °C
1200V; ASTM D4325
Dielectric Strength 730 kV/in96 hrs at 96% RH; ASTM D4325
 750 kV/inOriginal; ASTM D4325
 750 kV/in24 hrs in water; ASTM D4325
Dissipation Factor 0.70
@Frequency 60 Hz,
Temperature 23.0 °C
1200V; ASTM D4325
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.300 W/m-KASTM C518
Maximum Service Temperature, Air 90.0 °CContinuous
 130 °CEmergency Overload
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35185 / 169932

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.