Silpak SP-328-8 casting foam consists of two parts (A and B) that, after mixing, forms rigid or flexible foam product with densities of 8 lb/ft³. Consider SP-328-8 for production of decorative objects, lightweight mold shells, production parts, models, patterns, fixtures, duplicate masters and general tooling use. SP-328-8 is practically odorless and does not contain toluene diisocyanate, MOCA, heavy metals or HCFCs. Features: - Molded density of 8-20 lb/ft³.
- 1A:1B mix ratio by weight or volume
- Suitable for casting parts and filling voids
Applications: For production of: - Decorative objects
- Lightweight mold shells
- Production parts
- Models
- Patterns
- Fixtures
- General tooling use
Information provided by Silpak a division of Polytek Development Corp. |