MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Silpak SP-328-8 Rigid Polyurethane Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Silpak SP-328-8 casting foam consists of two parts (A and B) that, after mixing, forms rigid or flexible foam product with densities of 8 lb/ft³. Consider SP-328-8 for production of decorative objects, lightweight mold shells, production parts, models, patterns, fixtures, duplicate masters and general tooling use. SP-328-8 is practically odorless and does not contain toluene diisocyanate, MOCA, heavy metals or HCFCs.

Features:

  • Molded density of 8-20 lb/ft³.
  • 1A:1B mix ratio by weight or volume
  • Suitable for casting parts and filling voids
Applications: For production of:
  • Decorative objects
  • Lightweight mold shells
  • Production parts
  • Models
  • Patterns
  • Fixtures
  • General tooling use

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/galFree-Rise
 8.00 - 20.0 lb/galMolded
Viscosity 1100 cPMixed
Storage Temperature 60.0 - 90.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 minTack-Free Time
 10.0 - 15.0 minDemold Time
 45.0 secCream Time
 120 secRise Time
Shelf Life 6.00 Month
 
Descriptive Properties
Mix Ratio1A : 1Bby volume
 1A : 1Bby weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILPAK014 / 318651

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.