CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adhesion and flexibility, thermal stability, high conductivity, and superior peel strength. CHO-FLEX™ 601 coating can be sprayed or silkscreened, and will withstand wave solder temperatures above 500°F (260°C) without losing any of its exceptional properties Information provided by Chomerics |