MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-FLEX 601 Conductive Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adhesion and flexibility, thermal stability, high conductivity, and superior peel strength. CHO-FLEX™ 601 coating can be sprayed or silkscreened, and will withstand wave solder temperatures above 500°F (260°C) without losing any of its exceptional properties

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 g/cc
Solids Content 58 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00015 ohm-cm
@Thickness 0.0254 mm
film
Surface Resistivity per Square <= 0.050 ohm
@Thickness 0.0254 mm
film
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 107 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.0500 hour
@Temperature 260 °C
Wave Solder
 1.50 hour
@Temperature 182 °C
 5.00 hour
@Temperature 163 °C
Initial Cure
 90.0 hour
@Temperature 182 °C
Press Cycle
Shelf Life 6.00 Month
 
Descriptive Properties
Adhesion5BASTM D3359-78
BinderPolyurethane
ConsistencyThixotropic Paste
FillerAg
ResinPolyurethane
Theoretical Coverage4320 in2 / lbActual coverage will be 50-100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled
316 Stainless Steel, annealed sheet
Titanium Grade 2
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced
Silicon, Si

PCHOME071 / 28293

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.