MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials HYTEX® 700 Kevlar® Glass Industrial Textile
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemistry and in differing configurations (cloth, tape, sleeving, rope etc.). Mid-Mountain can design hybrid materials by blending most any combination of yarns.

HYTEX® 700 textile products are produced from blended yarns of Kevlar® and glass fibers. The blend combines the wear resistance of fiberglass with the tensile strength of Kevlar® to produce products with good strength and abrasion resistance at temperatures to 650ºF • 345ºC. Strength and dimensional stability are excellent while weight is low. HYTEX® 700 textiles are especially suited for use in heat shields, curtains, and various insulating applications.

Information provided by Mid-Mountain Materials.

Key Words: poly-paraphenylene terephthalamide, poly p-phenylene, aramid fiber, FRP composites
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 650 °FContinuous
 750 °FShort Term
Decomposition Temperature 800 °F
 
Descriptive Properties
Abrasion ResistanceGood
Acid ResistanceFair
Alkali ResistanceFair
ColorLight Yellow
CompositionKevlar® Glass Blend
Solvent ResistanceExcellent
Sunlight & Aging ResistanceFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials HYTEX® 400 Kevlar® Industrial Textile
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Isoflon Tisoflon® 5K Polytetrafluoroethylene Coated Kevlar Fabric
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
Lord Adhesives 310 High Strength SMC, FRP and General Purpose Epoxy Adhesive

PMID02 / 53085

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.