MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Applications: armor, belts, hoses, composite structures, cable sheathing, gaskets, brake pads, clutch linings, friction pads, slot insulation, phase barrier insulation, interturn insulation.

KEVLAR® is a DuPont registered trademark.

Key Words: poly-paraphenylene terephthalamide, poly p-phenylene, aramid fiber, FRP composites, single fiber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3450 MPa500000 psi
Modulus of Elasticity 179 GPa26000 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 425 °C797 °F
Decomposition Temperature 500 °C932 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber
E-Glass Fiber, Generic
Toyobo Dyneema® SK60 High Strength Polyethylene Fiber
DuPont™ Kevlar® Aramid Pulp

PCF003 / 27991

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.