MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Acetal Homopolymer, Unreinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.34 - 1.67 g/ccAverage value: 1.42 g/cc Grade Count:140
 1.14 - 1.19 g/cc
@Temperature 205 - 215 °C
Average value: 1.17 g/cc Grade Count:14
Water Absorption 0.0100 - 1.40 %Average value: 0.447 % Grade Count:40
Moisture Absorption at Equilibrium 0.100 - 0.900 %Average value: 0.286 % Grade Count:20
Water Absorption at Saturation 0.200 - 0.900 %Average value: 0.712 % Grade Count:8
Linear Mold Shrinkage 0.0100 - 0.0400 cm/cmAverage value: 0.0201 cm/cm Grade Count:101
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cmAverage value: 0.0185 cm/cm Grade Count:28
Melt Flow 1.00 - 70.0 g/10 minAverage value: 12.2 g/10 min Grade Count:111
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 50.0 - 95.0Average value: 87.7 Grade Count:30
Hardness, Rockwell R 78.0 - 122Average value: 114 Grade Count:32
Hardness, Shore D 76.0 - 86.0Average value: 82.7 Grade Count:7
Ball Indentation Hardness 150 - 175 MPaAverage value: 161 MPa Grade Count:5
Tensile Strength, Ultimate 45.0 - 75.8 MPaAverage value: 63.6 MPa Grade Count:42
 47.5738 - 47.5738 MPa
@Temperature >=71.1 °C
Average value: 47.6 MPa Grade Count:1
Tensile Strength, Yield 13.0 - 90.0 MPaAverage value: 66.7 MPa Grade Count:106
Elongation at Break 2.00 - 110 %Average value: 36.5 % Grade Count:131
Elongation at Yield 10.0 - 40.0 %Average value: 20.0 % Grade Count:27
Modulus of Elasticity 1.93 - 3.72 GPaAverage value: 3.01 GPa Grade Count:85
Flexural Yield Strength 37.9 - 267 MPaAverage value: 92.8 MPa Grade Count:72
Flexural Modulus 1.38 - 3.90 GPaAverage value: 2.80 GPa Grade Count:123
Compressive Yield Strength 14.0 - 114 MPaAverage value: 67.7 MPa Grade Count:12
Compressive Modulus 0.317 - 3.10 GPaAverage value: 2.15 GPa Grade Count:4
Poissons Ratio 0.370Average value: 0.370 Grade Count:21
Shear Strength 55.0 - 62.1 MPaAverage value: 60.3 MPa Grade Count:4
Izod Impact, Notched 0.374 - 12.8 J/cmAverage value: 1.03 J/cm Grade Count:67
 0.400 - 0.960 J/cm
@Temperature -40.0 - -29.0 °C
Average value: 0.620 J/cm Grade Count:3
Izod Impact, Unnotched 0.667 J/cm - NBAverage value: 6.01 J/cm Grade Count:7
Izod Impact, Notched (ISO) 7.00 - 10.0 kJ/m²Average value: 8.60 kJ/m² Grade Count:5
 7.00 - 8.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 7.67 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 250 - 250 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 250 kJ/m² Grade Count:1
Charpy Impact Unnotched 8.00 J/cm² - NBAverage value: 21.6 J/cm² Grade Count:24
 8.50 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 28.3 J/cm² Grade Count:17
Charpy Impact, Notched 0.400 - 1.60 J/cm²Average value: 0.918 J/cm² Grade Count:64
 0.400 - 1.30 J/cm²
@Temperature -40.0 - -30.0 °C
Average value: 0.860 J/cm² Grade Count:19
Gardner Impact 22.6 - 22.6 JAverage value: 22.6 J Grade Count:6
Tensile Impact Strength 98.1 - 358 kJ/m²Average value: 167 kJ/m² Grade Count:5
Coefficient of Friction 0.110 - 0.460Average value: 0.266 Grade Count:17
Coefficient of Friction, Static 0.140 - 0.450Average value: 0.224 Grade Count:7
Tensile Creep Modulus, 1 hour 2300 - 2900 MPaAverage value: 2740 MPa Grade Count:5
Tensile Creep Modulus, 1000 hours 1100 - 1600 MPaAverage value: 1500 MPa Grade Count:5
K (wear) Factor 11.1 - 403 x 10-8 mm³/N-MAverage value: 134 x 10-8 mm³/N-M Grade Count:4
Limiting Pressure Velocity 0.0513 - 0.160 MPa-m/secAverage value: 0.101 MPa-m/sec Grade Count:3
Taber Abrasion, mg/1000 Cycles 10.0 - 13.0Average value: 12.3 Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cmAverage value: 5.68e+14 ohm-cm Grade Count:24
Surface Resistance 1.00e+13 - 1.00e+16 ohmAverage value: 2.84e+15 ohm Grade Count:18
Dielectric Constant 3.10 - 4.10Average value: 3.74 Grade Count:23
Dielectric Strength 15.7 - 118 kV/mmAverage value: 30.6 kV/mm Grade Count:16
Dissipation Factor 0.00250 - 0.0100Average value: 0.00543 Grade Count:18
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:9
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.6 - 180 µm/m-°CAverage value: 104 µm/m-°C Grade Count:74
 99.0 - 99.0 µm/m-°C
@Temperature 22.8 - 55.0 °C
Average value: 99.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 95.0 - 120 µm/m-°CAverage value: 106 µm/m-°C Grade Count:16
Specific Heat Capacity 3.00 - 3.02 J/g-°C
@Temperature 215 - 215 °C
Average value: 3.01 J/g-°C Grade Count:3
Thermal Conductivity 0.230 - 0.375 W/m-KAverage value: 0.311 W/m-K Grade Count:11
 0.220 - 0.220 W/m-K
@Temperature 215 - 215 °C
Average value: 0.220 W/m-K Grade Count:2
Melting Point 157 - 180 °CAverage value: 174 °C Grade Count:71
Maximum Service Temperature, Air 80.0 - 150 °CAverage value: 104 °C Grade Count:17
Deflection Temperature at 0.46 MPa (66 psi) 124 - 340 °CAverage value: 163 °C Grade Count:97
Deflection Temperature at 1.8 MPa (264 psi) 78.8 - 277 °CAverage value: 107 °C Grade Count:135
Vicat Softening Point 148 - 180 °CAverage value: 160 °C Grade Count:6
Minimum Service Temperature, Air -50.0 °CAverage value: -50.0 °C Grade Count:4
Flammability, UL94 HBGrade Count:77
Flame Spread 20.0 - 80.0 mm/minAverage value: 28.5 mm/min Grade Count:13
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 - 300 °CAverage value: 227 °C Grade Count:8
Nozzle Temperature 188 - 216 °CAverage value: 195 °C Grade Count:5
Melt Temperature 177 - 230 °CAverage value: 205 °C Grade Count:55
Mold Temperature 40.0 - 121 °CAverage value: 83.8 °C Grade Count:57
Drying Temperature 71.1 - 121 °CAverage value: 83.2 °C Grade Count:54
Moisture Content 0.0500 - 0.200 %Average value: 0.184 % Grade Count:20
Injection Pressure 68.9 - 107 MPaAverage value: 88.3 MPa Grade Count:5
Vent Depth 0.00127 cmAverage value: 0.00127 cm Grade Count:3
Annealing Temperature 160 °CAverage value: 160 °C Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Overview of materials for Nylon 6, Extruded
Overview of materials for Acetal Copolymer, PTFE Filled
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade

O1280 / 77853

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.