MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Glass Fiber Reinforced

Material Notes: DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part performance under stress. Very good dimensional stability
  • Glass fibers offer stiffness but not reinforcement
  • Good machinabilityDELRIN®570 is used in a variety of industries such as automotive or construction where added strength and stiffness are desirable.

    Information provided by Ensinger

  • Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
    Density 1.49 g/cc0.0540 lb/in³ASTM D792
    Water Absorption 0.15 %
    @Time 86400 sec
    0.15 %
    @Time 24.0 hour
    ASTM D570
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell M 8181ASTM D785
    Tensile Strength, Yield 60.0 MPa8700 psiASTM D638
    Elongation at Yield 8.0 %8.0 %ASTM D638
    Tensile Modulus 4.65 GPa675 ksiASTM D638
    Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
     
    Electrical PropertiesMetricEnglishComments
    Surface Resistance 2.00e+15 ohm2.00e+15 ohmASTM D257
    Dielectric Constant 3.8
    @Frequency 1e+6 Hz
    3.8
    @Frequency 1e+6 Hz
    ASTM D150
    Dielectric Strength 17.8 kV/mm
    @Thickness 3.20 mm,
    Temperature 23.0 °C
    452 kV/in
    @Thickness 0.126 in,
    Temperature 73.4 °F
    ASTM D149
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 175 °C347 °FASTM D3418
    Maximum Service Temperature, Air 85.0 °C185 °Flong term
     149 °C300 °Fintermittent
    Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FASTM D648
    Flammability, UL94 HBHB

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Overview of materials for Acetal Homopolymer, Unreinforced
    Delrin Delrin® 570 NC000 POM-GF20
    Overview of materials for Nylon 6, Extruded
    Evonik Vestamid® L1600 nf (dry properties) Nylon 12
    Delrin Delrin® 525GR NC000 POM-GF25

    PENSIN097 / 122207

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.