MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Specialty Materials Boron Monofilament, 4 mil (102 µm) diameter
Categories: Metal; Other Engineering Material; Composite Fibers; Pure Element

Material Notes: Exceptional modulus and strength. The Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source. Elemental boron is deposited on a fine tungsten wire substrate and produced in diameters of 4.0-mil (102-micron) and 5.6-mil (142-micron). The resulting fiber is essentially amorphous boron with a fully borided-tungsten core. The textured surface provides an excellent interface in resin matrix composites, eliminating any need for sizing treatments. Primarily used in resin-matrix composites

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 3200
Tensile Strength, Ultimate 3600 MPa
Modulus of Elasticity 400 GPatension
Compressive Strength >= 6000 MPacalculated from composite lamina
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 25.0 W/m-Kbulk boron
Melting Point 2300 °C
Maximum Service Temperature, Air 500 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1350 °C
 
Component Elements PropertiesOriginal ValueComments
Boron, B 100 %
 
Descriptive Properties
Cross-SectionRound
Length> 7600 m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Aluminum, Al
DuPont™ Kevlar® 49 Aramid Fiber
Specialty Materials 5505 Boron Epoxy Prepreg Tape
Beijing Evergrow Resources BF-3 Basalt Needle Felt

NBORON00 / 15468

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.