MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema Kynar® 340 PVDF-CD
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.84 - 1.88 g/ccASTM D792
Density 1.78 g/ccISO 1183
Viscosity 2.50e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 3.0 - 8.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10.0 MPaDry; ISO 527-1/-2
Elongation at Break 40 %Dry; ISO 527-1/-2
Elongation at Yield 5.0 %Dry; ISO 527-1/-2
Tensile Modulus 1600 MPaDry; ISO 527-1/-2
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmDry; IEC 60093
Surface Resistance 10000 ohmCond.; IEC 60093
Dielectric Strength 27.0 kV/mmDry; IEC 60243-1
Dissipation Factor 0.070
@Frequency 100 Hz
Dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 166 °C10°C/min; Dry; ISO 11357-1/-3
 165 - 172 °CASTM D3418
Oxygen Index 43 %Dry; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 260 °C
Mold Temperature 23.0 - 90.0 °C
 
Descriptive Properties
ConductiveYes
Form as DeliveredGranules
Moisture SensitiveNo
Processing MethodsInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema Kynar® UHM 6020-20 PVDF-GF
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Arkema KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding

PARKF726 / 193527

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.