MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Kynar® UHM 6020-20 PVDF-GF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.87 - 1.89 g/cc1.87 - 1.89 g/ccASTM D792
Water Absorption 0.00 %0.00 %Dry; Sim. to ISO 62
Moisture Absorption 0.000 %0.000 %Dry; Sim. to ISO 62
Linear Mold Shrinkage 0.0025 - 0.010 cm/cm0.0025 - 0.010 in/inat 50% RH; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiDry; ISO 527-1/-2
Tensile Strength, Yield 120 MPa17400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
 3.0 %3.0 %Dry; ISO 527-1/-2
Tensile Modulus 0.788 GPa114 ksiASTM D638
 7.90 GPa1150 ksiDry; ISO 527-1/-2
Flexural Strength 174 MPa
@Strain 5.0 %
25200 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 6.56 GPa951 ksiASTM D790
Izod Impact, Notched 1.01 J/cm1.89 ft-lb/inASTM D256
Charpy Impact Unnotched 4.40 J/cm²
@Temperature 23.0 °C
20.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Tensile Creep Modulus, 1 hour 7900 MPa1.15e+6 psiCond.; ISO 899-1
Tensile Creep Modulus, 1000 hours 7900 MPa1.15e+6 psiCond.; ISO 899-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FDry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 35.0 µm/m-°C19.4 µin/in-°FDry; ISO 11359-1/-2
Melting Point 165 - 172 °C329 - 342 °FASTM D3418
 170 °C338 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 159 °C318 °FASTM D648
 159 °C318 °FDry; ISO 75-1/-2
Flammability, UL94 V-0V-0IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 °C446 °FInjection Molding; ISO 294
 230 - 250 °C446 - 482 °F
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °F
 60.0 °C140 °FInjection Molding; ISO 10724
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveNo
Processing MethodsInjection Molding
 Profile Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
Arkema Kynar® 340 PVDF-CD
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding

PARKF754 / 193546

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.