MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Conventus Polymers Duraflex TPU LCF30 BK 30% Carbon Long Fiber Reinforced, TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Duraflex TPU LCF30 BK is a long carbon fiber reinforced TPU for applications that require outstanding creep resistance, very high strength, low temperature impact, and dimensional stability. The natural grade is black.

Information provided by Conventus Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm0.00050 - 0.0010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0015 - 0.025 cm/cm0.0015 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 269 MPa39000 psiASTM D638
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %ASTM D638
Tensile Modulus 24.9 GPa3610 ksiASTM D638
Flexural Strength 389 MPa56400 psiASTM D790
Flexural Modulus 17.9 GPa2600 ksiASTM D790
Izod Impact, Notched 1.92 J/cm3.60 ft-lb/inASTM D256
Izod Impact, Unnotched 8.28 J/cm15.5 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 227 °C400 - 440 °F
Middle Barrel Temperature 210 - 232 °C410 - 450 °F
Front Barrel Temperature 216 - 238 °C420 - 460 °F
Melt Temperature 216 - 238 °C420 - 460 °F
Mold Temperature 93.3 °C200 °F
Injection Velocity 50.8 - 76.2 mm/sec2.00 - 3.00 in/sec
Drying Temperature 87.8 °C
@Time 14400 sec
190 °F
@Time 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Screw Speed 30 - 50 rpm30 - 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCONV937 / 233855

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.