MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Conventus Polymers Duraflex TPU LCF30 BK 30% Carbon Long Fiber Reinforced, TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Duraflex TPU LCF30 BK is a long carbon fiber reinforced TPU for applications that require outstanding creep resistance, very high strength, low temperature impact, and dimensional stability. The natural grade is black.

Information provided by Conventus Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0015 - 0.025 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 39000 psiASTM D638
Elongation at Break 1.0 - 2.0 %ASTM D638
Tensile Modulus 3.61e+6 psiASTM D638
Flexural Strength 56400 psiASTM D790
Flexural Modulus 2.60e+6 psiASTM D790
Izod Impact, Notched 3.60 ft-lb/inASTM D256
Izod Impact, Unnotched 15.5 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 185 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 440 °F
Middle Barrel Temperature 410 - 450 °F
Front Barrel Temperature 420 - 460 °F
Melt Temperature 420 - 460 °F
Mold Temperature 200 °F
Injection Velocity 2.00 - 3.00 in/sec
Drying Temperature 190 °F
@Time 14400 sec
Moisture Content <= 0.020 %
Back Pressure 25.0 - 50.0 psi
Screw Speed 30 - 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCONV937 / 233855

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.