MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Somos® WaterShed XC 11122 is the clear solution for numerous applications. Whether you’re a designer looking for highly detailed parts with superior clarity and water resistance, or an engineer focusing on durability for functional testing, Somos® WaterShed XC 11122 mimics the look and feel of clear thermoplastics, such as ABS and PBT. Somos® WaterShed XC 11122 produces optically clear parts with a smooth finish and it’s ease of use helps to shorten product development and testing. This versatility means Somos® WaterShed XC 11122 is the ideal material in markets such as automotive, aerospace and consumer electronics for applications including packaging, RTV patterns, durable concept models, wind tunnel testing and investment casting patterns.

Key Benefits:

  • Easy to use and finish
  • Superior moisture resistance
  • Exceptional clarity
Ideal Applications:
  • Consumer products
  • Fluid flow analysis
  • Duct work
  • Investment casting
  • Lenses

Information Provided by DSM Desotech Inc.

Vendors:
Available Properties
  • Density
  • Water Absorption, ASTM D570-98
  • Viscosity
  • Tensile Strength, Yield, ASTM D638M
  • Elongation at Break, ASTM D638M
  • Elongation at Yield, ASTM D638M
  • Modulus of Elasticity, ASTM D638M
  • Flexural Strength, ASTM D790M
  • Flexural Modulus, ASTM D790M
  • Izod Impact, Notched, ASTM D256A
  • Dielectric Constant, ASTM D150-98
  • Dielectric Constant, ASTM D150-98
  • Dielectric Constant, ASTM D150-98
  • Dielectric Strength, ASTM D149-97a
  • CTE, linear, ASTM E831-00
  • CTE, linear, ASTM E831-00
  • CTE, linear, ASTM E831-00
  • CTE, linear, ASTM E831-00
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648-98c
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648-98c
  • Glass Transition Temp, Tg, ASTM E1545-00
  • Refractive Index, ASTM D542
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.