MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sika Sikaflex® -2c NS Arctic Two-component, non-sag, polyurethane elastomeric sealant for arctic weather applications
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex 2c NS Arctic is a 2-component, premium-grade, polyurethane based, elastomeric sealant formulated for cold weather applications. It is principally a chemical cure in a non-sag consistency. Available in a wide range of architectural colors with convenient color paks. Meets ASTM C-920, Type M, Grade NS, Class 25, use T, NT, M, G, A, O and Federal Specification TT-S-00227E, Type II, Class A. Meets CAN/CGSB 19.24 - M90.

Where to use:

  • Intended for use in all properly designed working joints with a minimum depth of 1/4 inch.
  • Ideal for vertical and horizontal applications.
  • Adheres to most substrates commonly found in construction.
  • Mixable and placeable at temperatures as low as 15 F
  • Submerged environments, such as canal and reservoir joints.
  • An effective sealant for use in Exterior Insulation Finish Systems (EIFS).
Advantages:
  • Easy to mix, even at below freezing temperatures
  • Chemical cure allows the sealant to placed in greater depths for non-moving joints/cracks
  • High elasticity with a tough, durable, flexible consistency
  • Exceptional adhesion to most substrates without priming
  • Exceptional cut and tear resistance
  • Available in 35 standard architectural colors
  • Color uniformity via Color-pak system
  • Capable of +/- 50% Movement
  • Non-sag even in wide joints
  • Paintable with water, oil, and rubber based paints

Information provided by Sika Corporation.

Vendors:
Available Properties
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, Ultimate, ASTM C1135, H-piece
  • Tensile Strength, Ultimate, ASTM D412
  • Elongation at Break, ASTM C1135, H-Piece at Max. Load
  • Elongation at Break, ASTM C1135, H-piece
  • Elongation at Break, ASTM D412
  • Tear Strength, ASTM D624
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Final cure
  • Cure Time, Final cure
  • Cure Time, Final cure
  • Cure Time, Final cure
  • Tack-Free Time
  • Tack-Free Time
  • Shelf Life, in original unopened cartridge
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.