MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Materion Ta2O5 Tantalum Oxide for Optical Coating
Categories: Ceramic; Oxide

Material Notes: Tantalum pentoxide, Ta2O5, is a high-index, low-absorption material usable for coatings in the near-UV (350 nm) to IR (>8 µm) regions. Dense, hard layers can be deposited by electron-beam evaporation or by sputtering. Typical applications include near-UV to near-IR antireflection and multilayer filter coatings. Tantala can be used in combination with low-index Silicon dioxide layers to form high index-contrast multilayer structures ranging from wide-band AR coatings to bandpass filters and dichroic beam-splitters. That material combination is used to make thick multi-layer stacks that exhibit very low stress. An advantage over Titanium dioxide layers is the absence of absorption above 900 nm, making Tantala a superior material for near-IR laser and bandpass coatings such as Nd:YAG laser and telecom applications. Hard, scratch-resistant and adherent coatings can be deposited on glass and metal substrates. Films are also used for dielectrics in film capacitors and as gate insulators in large scale integrated circuits requiring low leakage voltage characteristics.

Information provided by Materion.

Vendors:
Available Properties
  • Density, Crystal
  • Molecular Weight
  • Melting Point
  • Refractive Index, without IAD
  • Refractive Index, without IAD
  • Refractive Index, without IAD
  • Refractive Index, without IAD
  • Refractive Index, without IAD
  • Refractive Index, With IAD
  • Refractive Index, With IAD
  • Refractive Index, With IAD
  • Refractive Index, without IAD
  • Refractive Index, without IAD
  • Refractive Index, With IAD
  • Refractive Index, With IAD
  • Refractive Index, With IAD
  • Refractive Index, With IAD
  • Refractive Index, without IAD
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Materion Corporation (former Williams Advanced Alloys)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.