Description Polypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding applications that require improved impact and clarity. Application PP 3479-01 is in compliance with the FDA requirements of 21 CFR 177.1520. Information provided by A. Schulman. |