MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: 316/316L UGIMA® is Ugitech’s improved machining grade. It is identical in every way to regular 316L, except with respect to machinability. Through modifications to the steel-making process, 316/316L UGIMA® builds upon the proprietary UGIMA® manufacturing process to allow for excellent machinability across a wider range of operations and cutting conditions. When compared with older Ugima® versions, 316/316L UGIMA® is a technologically advanced product that will allow for superior machinability at both low and high speeds, in cam-driven and CNC machines, and with high-speed steel or carbide tooling. Machine shops using 316/316L UGIMA® have experienced consistent success regardless of machine, operation, tooling, or cutting conditions. From lot to lot, 316/316L3 UGIMA® is engineered to give the same high performance every time.

Information provided by Schmolz + Bickenbach

Key Words: AISI316/316L; UNS S31600; UNS S31603; SAE J405 30316/30316L; 1.4401/1.4404, X2CrNimO17-12-2/X5CrNiMo17-12-2; ASTM A182; A193; A276; A314; A320; A479; A484; F899; ASME SA182; SA193; SA276; SA479; AMS 5648; AMS 5653; AMS-QQ-S-763; AMS-S-7720; MIL-S-862; NACE MR0175
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Turned Bars
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Turned Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Yield, Turned Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Elongation at Yield, Cold Drawn Bars
  • Elongation at Yield, Turned Bars
  • Reduction of Area, Cold Drawn Bars
  • Reduction of Area, Turned Bars
  • Tensile Modulus
  • Tensile Modulus
  • Tensile Modulus
  • Electrical Resistivity
  • Magnetic Permeability, at 23% cold work
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, followed by rapid cooling with forced air or water quenching
  • Hot-Working Temperature, Forge
  • Hot-Working Temperature, Forging range
  • Hot-Working Temperature, Heat in range
  • Hot-Working Temperature, Heat of core during fast forging
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.