MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NUCu Steel - ASTM A710 Grade B
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Northwestern University developed copper-precipitation-hardened, high-performance weathering steel that is produced by hot rolling after casting and then air-cooling. Due to simple processing the steel is fabricated at lower cost than competing high-performance steels that require quench and tempering. This steel can be easily welded without pre- or post-heating. The fracture toughness of the steel is excellent particularly at cryogenic temperatures. Weathering resistance and corrosion properties are better than that of any other available construction steel. The steel is included into ASTM A710 Standard. The steel is an excellent candidate for infrastructure applications such as bridges, posts, signs, railings, etc. as well as for applications in other fields.

Information provided by Professor Semyon Vaynman of Northwestern University.

Composition Notes: Composition as tested at Northwestern University.

Vendors:
Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, 2 inch gage specimen
  • Charpy Impact
  • Charpy Impact
  • Carbon, C
  • Copper, Cu
  • Iron, Fe, As Remainder
  • Manganese, Mn
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.