MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Teknor Apex SarlinkĀ® TPV 5765B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B series are highly engineered extrusion-grade thermoplastic vulcanizate with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a medium hardness, medium density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; High Heat Resistance; High Melt Stability; High Tensile Strength; Medium Density; Medium Hardness; Resilient; UV Resistant

Uses: Automotive Applications; Profiles; Rubber Replacement; Seals; Weatherstripping

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: BMW Mini/BMW Unspecified Color: Black; BMW Unspecified Color: Black; CHRYSLER MS-AR-100 BGV Color: Black; DAIMLER DBL 5562.30 Color: Black; FORD WSS-M2D379-B1; GM GMP.E/P.029; GM GMW15812P-TPV(EPMD+PP) Type 5E Color: Black; GM GMW15812P-TPV(EPMD+PP) Type 5M Color: Black; GM QK 003521 L Color: Black; HONDA Unspecified Color: Black; NISSAN NES M7075 Color: Black; PSA Peugeot-Citron B62 0300 version G Color: Black; RENAULT F.R.M 7A-10-A11 Color: Black; TOYOTA TSM 1707G-7 Color: Black; TOYOTA TSM 1707G-7 Color: Black; TOYOTA TSM 1707G-7 Color: Black; TOYOTA TSM 5746G-3 Color: Black; VAG VW501 23 Color: Black; VOLVO STD 318-06010 Color: Black

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Extrusion; Blow Molding

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ASTM D792
  • Viscosity, ASTM D3835, Shear, Capillary
  • Hardness, Shore A, ASTM D2240, Extruded
  • Hardness, Shore A, ASTM D2240, Injection Molded
  • Tensile Strength at Break, ASTM D412, Flow
  • Tensile Strength at Break, ASTM D412, Across Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Stress at Strain, ISO 37, Across Flow
  • Tensile Stress at Strain, ISO 37, Flow
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 1000 hr
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 168 hr
  • Elongation at Break, ASTM D412, Flow
  • Elongation at Break, ASTM D412, Across Flow
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked)
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • UL RTI, Electrical, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical without Impact, UL 746
  • Flammability, UL94, Black
  • Processing Temperature, Injection
  • Rear Barrel Temperature, Injection
  • Middle Barrel Temperature, Injection
  • Front Barrel Temperature, Injection
  • Nozzle Temperature, Injection
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 4, Extrusion
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  • Mold Temperature, Injection
  • Drying Temperature
  • Dry Time
  • Screw Speed, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.