MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Trinseo EMERGE™ PC 8130-6 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Product Description: EMERGE™ PC 8130-6 IC13000080 advanced resin is a translucent, ignition resistant PC resin that contains no chlorinated or brominated flame retardant additives and provides superior ignition resistance and ultraviolet light resistance. This resin combines good mechanical and high heat properties and maintains excellent processability and contains mold release agent.
Applications: Tube and build in LED lighting applications; Diffusers for lighting applications; Injection, extrusion or injection blow molded applications

Availability: Asia Pacific; Latin America; North America

Additive: Mold Release; UV Stabilizer

Features: Bromine Free; Chlorine Free; Flame Retardant; Good Processability; High Heat Resistance; Ignition Resistant; UV Resistant

Uses: LEDs; Lighting Applications; Sheet; Thin-walled Parts

Form: Pellets

Processing Method: Extrusion, Injection Blow Molding; Injection Molding

Information provided by Trinseo

Vendors:
Available Properties
  • Density, ASTM D792
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638, 2.0 in/min
  • Tensile Strength, Yield, ASTM D638, 2.0 in/min
  • Elongation at Break, ASTM D638, 2.0 in/min
  • Elongation at Yield, ASTM D638, 2.0 in/min
  • Tensile Modulus, ASTM D638, 0.039 in/min
  • Flexural Strength, ASTM D790, 0.051 in/min
  • Flexural Modulus, ASTM D790, 0.051 in/min
  • Izod Impact, Notched, ASTM D256
  • Arc Resistance, ASTM D495
  • CTE, linear, Parallel to Flow, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.