MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Lanxess Addocat® DB PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Product Information: Flexible slabstock foam (ester-based): Addocat DB is an activator for the production of flexible polyester foam based mainly on TDI 65/35. 1.0 - 1.6 parts by weight Addocat DB, calculated on 100 parts by weight polyester polyol, are used, depending on the water content of the formulation (2.0 - 5.0 parts by weight water). Since Addocat DB is insoluble in water, it can be emulsified in a mixture of water, Dispergiermittel WM and Zusatzmittel SM. Rigid polyurethane foam: Addocat DB slightly activates the crosslinking reaction. It is often used as a co-catalyst and gives rigid foam a tough and slightly elastic surface, especially in polyester-polyol containing systems.

Function: Catalyst for the production of polyurethane foams, e.g. ester-based flexible slabstock foam and rigid foam.

Applications:

  • Addocat DB is used mainly in the continuous production of slab-stock foam with densities higher than 50 kg/m³. Depending on the de-sired density, Zusatzmittel SM can be used simultaneously (at dosages of 1.0 - 4.0 parts by weight Zusatzmittel SM);
  • On-site casting
  • Continuous production of building boards with flexible and rigid or metal facings..

Information provided by Lanxess.

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Viscosity
  • Melting Point, Freezing Point
  • Boiling Point, Initial
  • Flash Point, DIN EN 22179
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.