MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chi Mei Wonderloy® PC-540A PC and ABS copolymer
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: High heat, halogen-free flame retardant, 1.5mm V-0, 2.0 mm 5VB. Applications: Set top boxes, projectors, computers, communication equipment, consumer electronics products, video game consoles, networking products.

WONDERLOY® PC alloy balances the properties of polycarbonate (PC) and acryloni-trile-butadiene-styrene copolymer (ABS). The PC component provides high heat resistance, high impact resistance, non-halogen flame retardancy, and high rigidity and tensile strength properties. The ABS component gives better processability, higher impact strength in low temperature environments, and the ability to be electroplated. WONDERLOY® PC Alloy offers lower specific gravity and delivers balanced mechanical properties, dimensional stability, and a high-quality appearance. This material effectively reduces the visible signs of injection, provides a wider range of injection conditions, and improves the maintenance rate for related equipment.

Information provided by Chi Mei Corporation

Vendors:
Available Properties
  • Density, ISO 1183
  • Linear Mold Shrinkage, ISO 294-4
  • Melt Flow, ISO 1133, Melt Volume Rate (ml/10 min.)
  • Spiral Flow, Chi Mei Test, V: 50%, P: 50%
  • Tensile Strength at Break, ISO 527, 50mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50mm/min
  • Flexural Strength, ISO 178, 2mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact, Notched, ISO 179, 1/8"
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • CTE, linear, ISO 11359
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/A, Unannealed
  • Vicat Softening Point, ISO 306, 50°C/hr
  • Vicat Softening Point, ISO 306, 50°C/hr
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chi Mei Corporation (ChiMei)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.