MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
Categories: Polymer; Thermoset; Epoxy

Material Notes: HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. The formulation has been designed to minimize chilling of the sheet and bring more material into the tool resulting in improved material distribution.

FLX may be used in plug applications with a wide range of polymer sheet material and provides easy machining and polishing plus very good curability. As compared to standard thermoset epoxy syntactics, FLX has nearly 3X the flexural toughness and more than 4X the elongation to break.

FLX has these outstanding attributes:

  • Minimal to no scratching
  • Good dimensional stability
  • Excellent toughness and durability
  • Good machinability
  • Temperature resistance
  • Low thermal conductivity

Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs.

Applications: HYTAC-FLX is a top choice for optical clarity with PET, provides excellent polymer yields as a result of better material distribution, lower starting gauge requirements and is more than double the flexural toughness of standard syntactic foams.

Recommended for use with APET, CPET, HIPS, OPS, PETG, PLA, PP, PVC and RPET.

Information Provided by CMT Materials, Inc.

Vendors:
Available Properties
  • Density
  • Flexural Toughness, ASTM D790
  • Compressive Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.