MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Thermal Ceramics V-19 Block Insulation
Categories: Ceramic

Material Notes: V-19 Block is manufactured from vermiculite granules and high-temperature bonding materials. This versatile product is available in thicknesses up to 4".

V-19 Block is an economical, energy saving insulation with minimal shrinkage at its top temperature limit, and good compressive strength. These features make V-19 a good design choice for back-up insulation applications.

V-19 compositional characteristics permits effective adhesion of cement finishes. Therm-O-Stix is an ideal adhesive product with superior qualities when used with V-19.

V-19 Block must be pre-drilled for placement since it is not impalable over anchors due to its high green strength. However this property makes it easy to cast or gun against with refractory castables.

Features:

  • Economical structural insulation
  • 1900°F (1038°C) temperature rating
  • Low thermal conductivity
  • No organic binders or fillers
  • Manufactured to close dimensional tolerances, max. ± 1/16”
  • Volumetric stable to use limit
  • Alternative to mineral wool board
  • Applications:

  • Back-up insulation in all industries
  • Suitable for use with castables, firebrick, refractory plastic and ceramic fiber

    Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

  • Vendors:
    Available Properties
    • Density, ASTM C303, at ambient temperature
    • Density, ASTM C303
    • Porosity, ASTM C493
    • Modulus of Rupture, ASTM C203, at ambient temperature
    • Modulus of Rupture, ASTM C203
    • Compressive Strength, ASTM C165, at ambient temperature
    • Compressive Strength, ASTM C165
    • Specific Heat Capacity
    • Thermal Conductivity
    • Thermal Conductivity
    • Thermal Conductivity
    • Maximum Service Temperature, Air, Continuous
    • Maximum Service Temperature, Air, Rating
    • Shrinkage, ASTM C356, Linear
    • Al2O3
    • Alkalis
    • CaO
    • Fe2O3
    • MgO
    • SiO2
    • TiO2
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.