MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tra-Con Tra-Cast FS407 Low Viscosity High Temperature Epoxy Casting System
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST FS407 is a low viscosity, solvent-free epoxy casting system recommended for rigid industrial laminating, electrical potting and transformer or coil embedding applications that require the effective combination of superior flow, good adhesion and excellent mechanical and electrical properties over a wide temperature range. This easy-to-use epoxy system has good wetting properties and develops excellent adhesion to glass, metals, ceramics, laminates and other high temperature resistant products. A final 90°C cure step is REQUIRED for complete cure. The fully cured casting system maintains a high volume resistivity, low coefficient of thermal expansion and good dimensional stability over a wide temperature range. In addition, its resistance to electrolysis, galvanic action and leakage offers protection against water, weather, gases and vapors, petroleum lubricants, fuels, salt solutions, mild acids, alkalis and many other organic and inorganic materials. An additional post-cure of 4 hours at 125°C is recommended when application temperatures higher than 125°C are anticipated.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Solids Content, Reactive Solids Content
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, 12hrs @ 25°C + 2hrs @ 65°C + 2 hrs @ 90°C
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.