MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Radel® R-5100 Polyphenylsulfone (PPSU), Opaque
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Opaque, general purpose for injection molding and extrusion

Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins. This resin also offers a high deflection temperature and outstanding resistance to environmental stress cracking. Radel® polymers are inherently flame retardant, provide excellent thermal stability and possess good electrical properties.

- Black: Radel® R-5100 BK937
- Bone: Radel® R-5100 NT15
- Grey: Radel® R-5100 GY1137
- Grey: Radel® R-5100 GY1037
- Grey: Radel® R-5100 GY874
- Blue: Radel® R-5100 BU1027

Markets/Uses: Aircraft / Aircraft Interiors / Extruded Profiles and Tubing; Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Parts/Thin Walls; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical Sheet Clear; Healthcare / Medical Devices / Medical Single Use Applications; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Sterilization Cases, Trays and Lids; Healthcare / Medical Devices / Surgical Instruments; Plumbing / Fittings & Manifolds / Fittings & Manifolds; Plumbing / Manifolds / Underfloor Heating

Applications: Aerospace Applications; Aircraft Applications; Connectors; Dental Applications; Food Service Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Plumbing Parts; Surgical Instruments

Features: Acid Resistant; Autoclave Sterilizable; Base Resistant; Biocompatible; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Flame Retardant; General Purpose; Good Sterilizability; Good Thermal Stability; Heat Sterilizable; High ESCR (Stress Crack Resist.); High Heat Resistance; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable; Ultra High Toughness

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Water Absorption, ISO 62
  • Moisture Absorption, ISO 62, 50% RH
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638
  • Tensile Stress, ISO 527-2
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Yield Strength, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Poissons Ratio, ASTM E132
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Tensile Impact Strength, ASTM D1822
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • CTE, linear, Parallel to Flow, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Glass Transition Temp, Tg, ASTM E1356
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Moisture Content, Injection
  • Back Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.